Wrist pin
Describe:
1.Material : 20 CrMnMo or 16MnCr5
2. Roughness EN ISO 1302:Ra6.3
3. Hardness before nitriding: 680 - 750 HV 0,5
4. Hardness after nitriding: min. 550 HV 0,5
5. (D) Nitride hardening depth: min. 15µm on final part
6 Tensile strenght
after quenching: Rm = 900 - 1350 N/mm²
after spheroidation: Rm max. = 500 N/mm²
7. Surface treatment: nitride hardening